Application:
To reduce nozzle clogging, calcium in steel after another, long strips of sulfide inclusions can be avoided. To improve the steel of anisotropy.
With the help of wire feeding machine, the steel liquid is rapidly input, melted and dissolved in the depth of the steel liquid, which plays the role of deoxidation, desulfurization and inclusion removal. At the same time, it can fine-tune the composition, improve the yield of metals and rare earth elements, and ensure the stability of the composition. Reduce the amount of precious elements, reduce the refining cost. It is suitable for calcium treatment of molten steel in the process of refining outside the furnace.
Ø13mm Suitable for medium and small electric furnaces.
Ø16mm Suitable for large electric furnace.
Size and shape;13土0.5mm,16土0.5mm
Ingredients:Ca≥30%,Fe≤70%
Diameter:13.5±0.5mm
Thick strip:0.4mm
Weight strip:170±10g/m
Content weight:≥250g/m
Wire weight:410-430g/m
Net weight:1.5T/volume
Length:3600-3750m/volume
Packing:Steel belt binding+waterproof plastic thin breast+external woven bag packaging+iron coating(paint)
Size of Line Volume:Internal diameter:590-600mm;outer diameter:1200-1300mm; width:6400mm,
Technical Parameter
Inquiry
Inquiry For More Information!Send Email To E-mail: info@fy-coredwire.com.com.Your email will be secreted totally,pls feel free to leave your email.
Popular Posts

Graphite Electrode
31-May-2019

Silicon Calcium Alloy
15-Apr-2019

Silicon-manganese Alloy
10-Apr-2019

Ferrosilicon Alloy
10-Apr-2019

Electrode Paste
20-Mar-2019

ECA/Electrically Calcined Anthracite
20-Mar-2019